Poor Drying

The paint film does not dry properly after the normal drying time and may require an extra-long drying period or not harden at all.

heikkokuivuminen

Cause:

  1. Incorrect mixing ratio for 2K paint (too much or too little hardener).
  2. Inappropriate hardener.
  3. Temperature does not reach the required level. Generally, if the temperature is below 10°C, the drying process slows down significantly.
  4. Excessive paint layer thickness.
  5. Poor weather conditions and inadequate ventilation.
  6. Insufficient, poor quality, or incorrect thinner.
  7. Incorrect application method.

Correction:

  1. Increase the drying temperature to ensure proper curing of the paint film.
  2. If the paint film does not dry properly even after increasing the temperature, sand or remove the paint and repaint.

Recommended products to prevent and fix potential issues:

<< BACK

Powered by Powered by